To make the PCB itself, he first coated a piece of copper clad board with black spray paint. Using the laser cutter at the makerspace, he was then able to blast away the paint, leaving behind the ...
Develop the board in Sodium Hydroxide solution (about 10 seconds). Rinse the board with clean water; Place in a heated etching tank of Ferric Chloride (15-45 minutes). This will remove unwanted ...